Abstract
Positron lifetime experiments of high statistical accuracy were performed for various polyethylene samples with different degrees of crystallinity (Xc = 43, 60, and 70%). Four lifetime components were resolved using the MELT, CONTIN or the discrete-term LIFSPECFIT routines. Two long-lived components appeared, their lifetimes and intensities varied systematically with Xc. τ4 arose from o-Ps annihilation in holes of the amorphous phase while τ3 may be attributed to crystals.
| Originalsprache | Englisch |
|---|---|
| Zeitschrift | Physica Status Solidi (A) Applied Research |
| Jahrgang | 172 |
| Ausgabenummer | 2 |
| Seiten (von - bis) | 303-315 |
| Seitenumfang | 13 |
| ISSN | 0031-8965 |
| DOIs | |
| Publikationsstatus | Veröffentlicht - 01.04.1999 |
UN SDGs
Dieser Output leistet einen Beitrag zu folgendem(n) Ziel(en) für nachhaltige Entwicklung
-
SDG 9 – Industrie, Innovation und Infrastruktur
Fingerprint
Untersuchen Sie die Forschungsthemen von „Do MELT or CONTIN programs accurately reveal the o-Ps lifetime distribution in polymers? II. Semicrystalline polymers“. Zusammen bilden sie einen einzigartigen Fingerprint.Zitieren
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver